Surface Analysis Of Internally Treated Dealkalized Containers

As received type II soda lime glass containers were investigated with SIMS, XPS, EMPA and IRRS to assess the chemical composition of the inner surface and the type and depth of the dealkalization profiles produced by surface treatment. The analysis of a range of samples produced with various processes showed that the composition of the outer 5nm is similar, while the dealkalization level and the profile depth vary from sample to sample and within a given container, as a result of the process conditions. The bloom consists essentially of crystalline sodium sulfate, occasionally associated with some bisulfate.

Author
M Verita Et Al
Origin
Staz Per Vetro, Italy
Journal Title
Fundamentals Glass Science & Technol 1997 174-180
Sector
Special Glass
Class
S 2562

Request article (free for British Glass members)

Surface Analysis Of Internally Treated Dealkalized Containers
Fundamentals Glass Science & Technol 1997 174-180
S 2562
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
17 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.