Surface Analysis Of 24% Lead Crystal Glass Articles: Correlation With Lead Release

The surface of unused lead crystal wine goblets before and after acetic acid extraction tests was analysed with the surface analytical techniques electron problem microanalysis (EPMA), X-ray photoelectron spectroscopy (XPS) and secondary ion mass spectrometry (SIMS). The release of lead was determined by 24h extraction tests with 4% acetic acid at room temperature, preparing the samples in two conditions: unwashed (as received, formed and stored for 6 months) and washed with water. Lead release in the first 5 minutes was 50% of the 24h release. 24h lead release decreased by about 20% after washing. Pb release from samples exposed to a second or third acetic acid extraction test was a small fraction of the initial one.

Author
E Guadagnino Et Al
Origin
Stazione Sperimental, Italy
Journal Title
Glass Technology 43 2 2002 63-69
Sector
Domestic glass
Class
D 605

Request article (free for British Glass members)

Surface Analysis Of 24% Lead Crystal Glass Articles: Correlation With Lead Release
Glass Technology 43 2 2002 63-69
D 605
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
18 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.