Superconducting Properties Of Barium-Doped (Bi,Pb)2Sr2Ca2Cu3Ox Glass-Ceramics

The Ba-doped, superconducting (Bi,Pb)2Sr(2-x) BaxCa2Cu3Oy and (Bi,Pb)2Sr2Ca(2-x)BaxCu3Oy (0 x 1.0) were prepared by using a melt-quenching method, and the effect of Ba additions on the glass forming ability and the crystalline phase was examined.