Superconducting Coupling Nature At Grain Boundaries In Bisr2Cacu2Ox Glass-Ceramics

Superconducting coupling nature at grain boundaries in bismuth strontium calcium copper oxide glass-ceramics consisting mainly of the low-Tc phase was examined by measuring superconducting properties and temperature or ac field dependence of ac complex susceptibility.