Sulphur Functioning During Glass Melting

The impact of sulphur compounds on the sand dissolution process and foaming was investigated in the model soda-lime-silica glass with the additions of carbon and sulphate in molar ratios 0-6. The aim of the work was to test the mentioned fining combination for the role of chemical accelorator of glass melting. The sulphate with carbon proved acceleration of the sand dissolution at 1300C but the results at lower temperatures were less convincing. The volume foaming was observed and evaluated in slightly reduced and reduced glasses at 1300-1400C the bubble nucleation, rapid growth and foam formation on the glass level in contact with water vapour atmosphere was attributed to chemical reaction between water vapour and sulphur compounds in the melt.

Author
A. Miroslava Et Al
Origin
Institute Of Inorganic Chemisrty, Rez, Czech Republic.
Journal Title
Advanced Materials Research Vols 39-40 (2008) 413-418
Sector
General
Class
G 3522b

Request article (free for British Glass members)

Sulphur Functioning During Glass Melting
Advanced Materials Research Vols 39-40 (2008) 413-418
G 3522b
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.