Subcritical Crack Growth In A Phosphate Laser Glass

The rate of subcritical crack growth in a metaphosphate Nd-doped laser glass was measured using the double-cleavage-drilled compression (DCDC) method.

Author
S N Crichton Et Al
Origin
Rensselaer Polytechnic, New York, Usa
Journal Title
J Am Ceram Soc 82 11 1999 3097-3104
Sector
Special Glass
Class
S 1753