A Study On Zns Long Afterglow Fluorescent Glass Coating

Fluorescent glass coatings have been obtained by taking ZnS:Cu, Cl long afterglow fluorescent materials, doped Er3+, Gd3+ as fluorescent substances, Si02-B203-RO-R20 low melting glass as matrix. The crystalline phases in the coatings are investigated by XRD, SEM and XPS. The results indicate that there are a large number of ZnS crystals and a minor amount of Zn0 crystals in the pure fluorescent materials - besides the above-mentioned two crystals there is also a minor amount of Zn-S04 crystals. The study of XPS displays that the crystalline group only consists of ZnS crystals, which confirms that the crystalline groups do not react to glass.

Author
W Cehngyu Et Al
Origin
Dalian Inst Of Light Industry, China
Journal Title
Proc 17Th Int Cong Glass, Beijing, Vol 3 October 1995 687-692
Sector
Special Glass
Class
S 1301

Request article (free for British Glass members)

A Study On Zns Long Afterglow Fluorescent Glass Coating
Proc 17Th Int Cong Glass, Beijing, Vol 3 October 1995 687-692
S 1301
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.