Study Of Silver Diffusion Kinetics In Ion Exchange Photochromic Glass

The silver diffusion process is an important factor affecting the properties of ion exchange photochromic glass. This paper studies the diffusion at the glass/salt bath interface, approximately calculates the silver self diffusion coefficient and re-examines the concentration profiles of silver.