A Study Of Physicochemical Phenomena In Evaluation Of Chemical Corrosion In Glass

The process of chemical corrosion of glass is investigated using a methylene blue indicator.Kinetic and concentration dependences for absorption of the colorant by silica acid gel are obtained, including the process on the bottle inner surface. Causes and the mechanism of origin of sediments in vodka are discussed, and practical measures preventing sediment formation are proposed.

Author
Yu A Guloyan Etal
Origin
Research And Development Institute Of Glass, Moscow, Russia.
Journal Title
Glass And Ceramics 57 7-8 2000 267 - 272
Sector
Special Glass
Class
S 3173

Request article (free for British Glass members)

A Study Of Physicochemical Phenomena In Evaluation Of Chemical Corrosion In Glass
Glass And Ceramics 57 7-8 2000 267 - 272
S 3173
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.