Study On Lead Leaching From Crystal Glass In Different Conditions (In Chinese)

Three lead crystal glass samples with different Pb3O4 content were prepared and the samples dipped in white spirit and detergent at 80 deg C was studied. The lead leaching rate and surface morphology of corroded lead crystal glass were measured by: weight loss method; optical microscopy; and inductively coupled plasma mass spectrometry. The results show that the lead crystal glass soaked in different solutions for several days will lead to the leaching of lead, and the leaching rate will depend on the Pb3O4 content in the samples.

Author
L Luo Et Al
Origin
Donghua University, Shanghai, China
Journal Title
Glass & Enamel 46 2 April 2018 2-5
Sector
Domestic glass
Class
D 1419

Request article (free for British Glass members)

Study On Lead Leaching From Crystal Glass In Different Conditions (In Chinese)
Glass & Enamel 46 2 April 2018 2-5
D 1419
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.