A Study Into The Interaction Of Improted Wine Bottles And The Uk'S Cullet Supply

This study was commissioned by WRAP, which was established to promote sustainable waste management. WRAP identified that the trade in wine was a major contributor to the domestic waste stream and colour imbalance. The study has quantified these contributions and analysed the implications of various actions that could be encouraged to improve the utilisation of waste glass; in particular those measures that would allow the glass to be recycled through the melting furnace, which is considered to be the best environmental option. For more information please see: www.wrap.org.uk/retail/materials/glassrite_wine.html

Author
Un-named
Origin
Unknown
Journal Title
Gla0059 Isbn 1844052303 January 2006
Sector
Container glass
Class
C 3594

Request article (free for British Glass members)

A Study Into The Interaction Of Improted Wine Bottles And The Uk'S Cullet Supply
Gla0059 Isbn 1844052303 January 2006
C 3594
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.