Study Of High-Temperature Spectral Behaviour Of Container Glass

Spectral absorption coefficients of container glasses in the wavelength from 0.4 to 4.5um and in the temperature range from room temperature to 1400 deg C were measured by a single-beam spectrophotometer by means of the transmission method. From the measured absorption coefficients radiative thermal conductivities in the temperature range from 600 to 1400 deg C were calculated by means of Rosselund's diffusion approximaiton. The intensity of the band at 2.8um due to dissolved hydroxyl groups in glass was also calculated.

Author
J Endrys Et Al
Origin
Inst Chem Tech, Prague, Czech Republic
Journal Title
Glastech Ber Glass Sci Technol 70 5 1997 126-136
Sector
Container glass
Class
C 1047

Request article (free for British Glass members)

Study Of High-Temperature Spectral Behaviour Of Container Glass
Glastech Ber Glass Sci Technol 70 5 1997 126-136
C 1047
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.