Study Of Corrosion Processes In Glass By A Multitechnique Approach. Part 1. Atomic Absorption Spectroscopy, Atomic Emission Spectroscopy And Scanning Electron Microscopy

The kinetics of the reaction of four types of glasses (with medieval composition) with water and aqueous solutions of pH2 and 4 were studied by exposing a well defined surface area of glass samples to the leaching solutions under static conditions. The results show that a selective leaching of alkali ions took place.

Author
A A Salem Et Al
Origin
Univ Of Vienna, Austria
Journal Title
Glass Technology 35 2 1994 89-96
Sector
Special Glass
Class
S 797

Request article (free for British Glass members)

Study Of Corrosion Processes In Glass By A Multitechnique Approach. Part 1. Atomic Absorption Spectroscopy, Atomic Emission Spectroscopy And Scanning Electron Microscopy
Glass Technology 35 2 1994 89-96
S 797
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.