A Study On The Classification Of The Bubbles In Glass Using Modern Techniques

The author studied the classification of 300 bubbles using modern techniques. First, the appearance of the bubbles were observed under the optical microscope then, the bubbles were classified according to the kinds of inclusions in the bubbles. The solid inclusions in the bubbles were analysed using nondestructive analysis techniques, viz. laser Raman probe microzone analyser, and a section of the bubble was analysed using an electron probe analyser.

Author
G Minqin Et Al
Origin
Unknown
Journal Title
Proc 17Th Int Cong Glass Vol 3, Oct 1995 677-681
Sector
General
Class
G 1697

Request article (free for British Glass members)

A Study On The Classification Of The Bubbles In Glass Using Modern Techniques
Proc 17Th Int Cong Glass Vol 3, Oct 1995 677-681
G 1697
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.