The Study And Analysis Of The Strucutre Of Foam Glass

Measurements and microscope observations have been made on the structural elements of foam glass. Six structural elements are distinguished and their distribution on the surface and in the bulk glass have been determined. It is concluded that there is a regular distribution of the structural elements of foam glass.