Structure Of Te02.Zn0 Glasses By Rdf And Te, Zn, K Exafs

Using synchrotron radiation, structure of Te02.Zn0 glasses with three different Zn0 contents (15, 25 and 35 mol%) are investigated by x-ray diffraction.