Structure Study Of Sol-Gel Derived Sodium Germanate Glasses By X-Ray Diffraction And Exafs Methods

The xNa20.(100-x)Ge02(x=10, 15, 20 mol%) glasses were prepared by the sol-gel method from sodium methoxide and germanium butoxide. The structure of the glasses was investigated by means of x-ray radial distribution function and EXAFS analyses and was compared with that of the corresponding melt derived glasses. It was found that the mode of formation of glasses affects the glass structure, and the fraction of sixfold coordinated Ge4+ ions, N6 in the sol-gel derived glasses is almost twice as large as the melt derived ones. The clustering of Ge06 octahedra in the sol-gel derived glasses to form a group such as [Ge4016]4- found in Na4Ge9020 crystal was proposed. The sol-gel derived glasses were crystallised at lower temperatures than the melt derived ones.

Author
K Kamiya Et Al
Origin
Mie University, Japan
Journal Title
Phys Chem Glasses 39 1 1998 9-16
Sector
Special Glass
Class
S 1344

Request article (free for British Glass members)

Structure Study Of Sol-Gel Derived Sodium Germanate Glasses By X-Ray Diffraction And Exafs Methods
Phys Chem Glasses 39 1 1998 9-16
S 1344
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.