Structure Of Sodium Aluminosilicate Glasses

A series of sodium aluminosilicate glasses composed of varying alumina/soda ratios has been simulated with the molecular dynamics technique using a tetrahedral form of a three-body interaction potential.

Author
D M Zirl, S H Garofalini
Origin
Rutgers University
Journal Title
J Am Ceram Soc 1990 73 10 2848-2856
Sector
Special Glass
Class
S 470