Structure Evolution And Optical Properties Of Co-Doped Zinc Aluminosilicate Glass-Ceramics

Temperature induced structure evolution of zinc aluminosilicate glasses nucleated by TiO2 and doped with cobalt oxide was studied by small angle x-ray scattering, x-ray diffraction analysis, Raman and optical spectroscopy. According to the SAXS data, the phase separation by spinodal decomposition that occurred during glass melt cooling and annealing proceeded upon further heat-treatments. Cobalt oxide facilitated amorphous phase separation of the parent glass that resulted information of a cobalt-doped amorphous zinc aluminotitanate phase and gahnite, ZnAl2O4, cyrstals. Cobalt-doped gahnite nanometer sized crystals were formed at temperatures as low as 720 deg C and remained the only crystalline phase if heat treatment temperature did not exceed 950 deg C.

Author
I Alekseeva Et Al
Origin
Vavilov State Optical Institute, St Petersburg, Russia
Journal Title
Phys Chem Glasses Eur J Glass Sci Technol 53 4 2012 167-180
Sector
Glass Ceramics
Class
GC 820

Request article (free for British Glass members)

Structure Evolution And Optical Properties Of Co-Doped Zinc Aluminosilicate Glass-Ceramics
Phys Chem Glasses Eur J Glass Sci Technol 53 4 2012 167-180
GC 820
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
16 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.