The Structure Of Cao-Na20-Mg0-P205 Invert Glass

Besides phosphate-containing biocompatible glass ceramics, vitreous bone implants have received attention in recent years. Glasses of the system CaO-Na2O-MgO-P2O5 were used of the development of porous, resorbable implant material. These glasses represent polyphosphates containing

Author
G Walter Et Al
Origin
Rostock University, Germany
Journal Title
Proc Icg Extended Abstracts 2 2001 146-147
Sector
Special Glass
Class
S 2648