The Structure And Phase Transitions In Aluminosilicate Glasses And Melts

After silica, aluminium oxide is one of the most important components of both natural and technical glasses and melts. All industrial glasses contain aluminium oxide to some extent and its influence on glass properties is rather considerable. There are many works on the structural state of aluminium ions in glass and a brief statement of the main results is given in this paper.

Author
B G Varshal
Origin
State Glass Research Institute, Moscow
Journal Title
Fundamentals Of The Glass Manufacturing Process 1991. Esg Conf. 76-80
Sector
Special Glass
Class
S 778

Request article (free for British Glass members)

The Structure And Phase Transitions In Aluminosilicate Glasses And Melts
Fundamentals Of The Glass Manufacturing Process 1991. Esg Conf. 76-80
S 778
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.