Structure And Nonlinear Optical Properties Of Lanthanide Borate Glasses

The third-order nonlinear optical susceptibility, X(3), of lanthanide (lanthanum, praseodymium, neodymium, and samarium) borate glasses has been measured the third harmonic generation method.

Author
K Terashima Et Al
Origin
Kyoto University, Japan
Journal Title
J Am Ceram Soc 80 11 1997 2903-2909