Structure And Nonlinear Optical Properties Of Pb0-Bi203-B203 Glasses

The third order nonlinear optical susceptibilities X(3) of Pb0-Bi203-B203 glasses have been measured by the third harmonic generation (THG) method. The borate network structure in the present glass system has also been investigated by using Raman and 11B MAS NMR spectroscopies.