Structural Studies Of Metaphosphate Glasses Using Small Angle X-Ray Scattering Techniques

A series of metaphosphate glasses was investigated by small angle X-ray scattering techniques to extract information on their microstructure and short and intermediate range order.

Author
G Walter Et Al
Origin
University Rostock, Friedrich Schiller University Jena
Journal Title
Phys Chem Glasses 1990 31 5 188-195
Sector
Special Glass
Class
S 447