A Structural Investigation Of High Alumina Glasses In The Cao-Al2O3-Sio2 System Via Raman And Magic Angle Spinning Nuclear Magnetic Resonance Spectroscopy

Calcium aluminosilicate glasses with compositions CaO:Al2O3=1 and CaO:Al2O3

Author
R K Sato Et Al
Origin
Arizona State University, University Of Warwick
Journal Title
Phys Chem Glasses 1991 32 4 149-156