The Structural Diversity Of The Nanoworld

The structural diversity of the nanoworld and its origin are analysed. Consideration is given to different aspects of this problem, such as the non equilibrium, coherence, hierarchic structure, fragmentation, and generalised symmetry. Inhomogeniety of the structure of a nanoparticle and structural diversity of the nanoworld are treated as a result of the self organisation of a non equilibrium nonlinear multivariant system.

Author
V Y Shevchenko Et Al
Origin
Unknown