Structural, Dielectric And Optical Properties Of Srb407-Ba0-Ti02 Glasses

Glass samples with compositions (100-2x)SrB407-xBa0-xTi02 were prepared by conventional melt quenching and the influence of the addition of Ba0-Ti02 on the strucutral, dielectric and optical properties of SB0 glasses was studied.

Author
M V Shankar & K B R Varma
Origin
Indian Inst Of Science, Bangalore, India
Journal Title
Phys Chem Glasses 40 1 1999 44-47
Sector
Special Glass
Class
S 1647