Structural And Optical Properties Of Nickel Zinc Alumino-Gallo-Silicate Glass

Transparent glass-ceramic was obtained from ZnO-Ga2O3-Al2O3-SiO2 glasses. The colour drastically changed from brownish yellow to green on heat treatment between the glass transition and crystallisation temperatures. The crystalline phase precipitated in the treatment was identified as spinel type crystal, by x-ray diffraction measurements. Transmission electron microscope observations confirmed that the crystalline size was about 10-15nm in diameter. Broadband near-infrared emission was observed from the transparent glass-ceramic with the excitation by 976nm. It was thought that the spinel nano-crystallites containing Ni should act as the emission centre.

Author
T Suzuki Et Al
Origin
Toyota Tech Inst, Japan
Journal Title
9Th Int Conf Corning - Phys Chem Glasses 46 4 2005 400-403
Sector
Glass Ceramics
Class
GC 653

Request article (free for British Glass members)

Structural And Optical Properties Of Nickel Zinc Alumino-Gallo-Silicate Glass
9Th Int Conf Corning - Phys Chem Glasses 46 4 2005 400-403
GC 653
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 14 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.