Strong And Chemically Inert Sinter Crystallised Glass Ceramics Based On Estonian Oil Shale Ash

In heat and power production, oil shale combustion forms substantial amounts of solid waste, including fly ash. This paper is dedicated to the manufacturing of frit derived glass ceramics from melting high amounts of this waste (65-67 wt%) combined with inexpensive minerals such as rhyolite (33-35 wt%). Owing to a surface mechanism of crystallisation, fine powders led to glass ceramics with high strength and reliability, even for rapid treatments (fast heating, at a rate of 40 dec C min-1, followed by 30 min holding stage). To minimise the presence of pressing and de-molding induced defects, the tiles were prepared by incorporating binders, i.e. polyethylene glycol or kaolin, to the frit mixtures. Finally, the stabilising effect of recycled borosilicate glass powders, mixed with waste derived glass powders, was also investigated with promising results for the production of a chemically stable material.

Author
M Marangoni Et Al
Origin
University Padova, Italy
Journal Title
Advances In Applied Ceramics 113 2 2014 120-128
Sector
Glass Ceramics
Class
GC 875

Request article (free for British Glass members)

Strong And Chemically Inert Sinter Crystallised Glass Ceramics Based On Estonian Oil Shale Ash
Advances In Applied Ceramics 113 2 2014 120-128
GC 875
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.