Stress-Strain State Of Fibre Bundles In Glass-Fibre-Reinforced Concrete Structural Elements

The stress-strain diagrams of glass-fibre bundles working in tension are analyzed. The results for glass fibres in normal conditions and for glass fibres soaked in a saturated Ca(OH)2 solution (to mimic a concrete or cement binder medium) are compared.