Stress Prediction And Measurement In Chemical Toughening

The interaction between stress development due to diffusive ion exchange and viscoelastic stress relaxation is discussed and a specific model is described. In some circumstances the peak stress is expected to occur below rather than at the surface. Stress measurement techniques using the waveguide effect in the surface layers become unreliable when this is the case. Modelling of the direct and inverse waveguide problems is used to explore the behaviour of a particular measurement technique.

Author
D Gelder Et Al
Origin
Pilkington Technology Centre
Journal Title
Fundamentals Of The Glass Manufacturing Process 1991.Esg Conf. 104-107
Sector
General
Class
G 1036

Request article (free for British Glass members)

Stress Prediction And Measurement In Chemical Toughening
Fundamentals Of The Glass Manufacturing Process 1991.Esg Conf. 104-107
G 1036
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.