Stress Generation Modulus As A Counterpart Of The Stress Relaxation Modulus

In order to measure the time dependence of the stress relaxation modulus, E, a stress-strain deformation has to precede which induces a stress within the viscoelastic sample from which the sample relaxes. The generation of stress is characterised by a strain rate-dependent and relaxation rate-dependent portion which exhibits a maximum value, Emax, which is called "stress generation modulus". Emax was called the "maximum stress relaxation modulus" in earlier papers, however, a better verbal distinction has been made by the new term because Emax is about one order of magnitude larger than E.

Author
R Bruckner Et Al
Origin
Inst Fur Nichmetallische Werkstoffe, Germany
Journal Title
Glastech Ber Glass Sci Technol 68 2 1995 70-72
Sector
General
Class
G 1204

Request article (free for British Glass members)

Stress Generation Modulus As A Counterpart Of The Stress Relaxation Modulus
Glastech Ber Glass Sci Technol 68 2 1995 70-72
G 1204
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
18 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.