Stress And Strain Evolution In Cast Refractory Blocks During Cooling

A computational model has been developed to study the stress and strain histories experienced by zirconia-containing cast refractory blocks when they are cooled from the casting temperature.

Author
T J Lu Et Al
Origin
Cambridge University, Uk
Journal Title
J Am Ceram Soc 81 4 1998 917-925
Sector
Refractories
Class
R 269

Request article (free for British Glass members)

Stress And Strain Evolution In Cast Refractory Blocks During Cooling
J Am Ceram Soc 81 4 1998 917-925
R 269