The Strengthening Of Some Commercial Ophthalmic And Filter Glasses By Ion Exchange

The strengthening of various glasses by ion exchange at different temperatures in molten potassium nitrate or a solution of molten potassium nitrate and sodium nitrate is examined.

Author
J S Stroud
Origin
Schott Glass Technologies Inc
Journal Title
Glass Technology 1988 29 3 108-114