Strength Of Silicon Nitride After Thermal Shock

A water-quenching technique was used to evaluate the thermal-shock strength behaviour of silicon nitride ceramics in an air atmosphere. When the tensile surface was shielded from air during the heating and soaking process, the quenched specimens showed a gradual decrease in strength at temperatures above 600 deg C. However, the specimens with the air-exposed surface exhibited a ~16% and ~29% increase in strength after quenching from 800 and 1000 deg C, respectively. This is because of the occurrence of surface oxidation, which may cause the healing of surface cracks and the generation of surface compressive stresses. As a result, some pre-oxidation of Si3N4 components before exposure to a thermal-shock environment is recommended in practical applications.

Author
J She Et Al
Origin
Aist, Japan
Journal Title
Jacs 86 9 2003 1619-1621
Sector
Special Glass
Class
S 2577

Request article (free for British Glass members)

Strength Of Silicon Nitride After Thermal Shock
Jacs 86 9 2003 1619-1621
S 2577
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.