The Strength Of Silicate Glasses: What Do We Know, What Do We Need To Know?

In the last few years, there has been increased interest in methods to improve the practical strength of inorganic glasses. During this same time frame, new theoretical and experimental techniques have appeared. In this paper, we discuss this interest and indicate how and where these new techniques may help to achieve objectives to increase the practical strength of glass.

Author
C R Kurkjian Et Al
Origin
University Southern Maine, Usa
Journal Title
Int J Applied Glass Science 1 1 2010 27-37