Strength Levels Of Flat Glasses

The strength of industrial flat glasses and glassware depends on the presence of defects in their surface layer. Studies have shown that the experimentally obtained strength values of industrial glasses usually group around certain distinct values that are determined by the presence of different types of defects at the surface of the glasses.