Strength And Fracture Of Glass

Relationships between structural strength, ultimate deformation and polymerization degree of anionic network of glass are considered in this paper. The description of fatigue fracture of glass using exponential and power functions is analysed. The physical sense of glass fatigue process is well expressed by exponential form.