Strength And Fatigue Of Float Glass Before And After Enameling

Biaxial flexure test methods were used to interrogate the role of tin penetration and enamelling on the strength and dynamic fatigue behaviour of float glass. A twofold higher strength was observed for the air versus tin side of unenamalled float glass and was attributed to differences in flaw severity and population between the two surfaces. The tin side contained significantly larger flaws than the air side, presumably due to damage induced by contact with the rollers in the aft end of the float process line. The strength of the enamelled float glass is significantly lower than the un enamelled glass, independent of the side to which the enamel is applied. Fracture in the enamelled float glasses initiates from defects, such as pores, pigment aggregates and un-fused reagents that are contained in the enamel.

Author
M H Krohn Et Al
Origin
Unknown
Journal Title
The Glass Researcher 11 2 2002 24-28
Sector
Flat glass
Class
F 1336

Request article (free for British Glass members)

Strength And Fatigue Of Float Glass Before And After Enameling
The Glass Researcher 11 2 2002 24-28
F 1336
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.