Statistics In The Batch Plant

A glass batch plant offers a wonderful opportunity to use statistics to keep the batch making process operating within prescribed limits. Different portions of the batch system can also be studied to improve the process of the batch system. This paper looks at statistical control, which means that the process is operating within the limits of the historical distribution of the variables in question, in this instance, raw material weighments. It is presumed that these limits are within the customer specifications.