Statistical Experimental Design For Refractory Coatings

The application of paint to a substrate, processing of some food items, manufacture of many cosmetic products, and application of refractory coatings on metal casting moulds all depend on the development of suitable rheological characteristics, such as viscosity and thixotropy, in the product. In practice, the optimisation of composition, in terms of both rheological behaviour and final properties, often is found by trial-and-error, which can be quite expensive and time consuming. A more efficient approach is to use a statistical model to evaluate the effects of composition on rheology and other properties. In this paper, the basic concepts of mixture design and analysis are applied to the formulation of a refractory coating, with illustration by a worked example. Experimental data of coating viscosity vs composition are fitted to the model.

Author
J A Mckinnon Et Al
Origin
University Of New South Wales, Sydney
Journal Title
J Aust Ceram Soc 36 2 2000 59-63
Sector
Refractories
Class
R 387

Request article (free for British Glass members)

Statistical Experimental Design For Refractory Coatings
J Aust Ceram Soc 36 2 2000 59-63
R 387
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.