State-Of-The-Art Electrically Ordered Chromogenic Devices For Glazing Applications (In Italian)

Two families of chromogenic materials (liquid crystals and electrochromics) are examined for their possible application in the production of glazing which is able to commute in a reversible way, either from a transparent to a diffusing state (liquid crystal), or from a transparent to a coloured state (electrochromic).