Spiraling Glass Fibres

By twisting fibre-optic strands into helical shapes, researchers at Chiral Photonics Inc have created unique structures that can precisely filter, polarize or scatter light. Compatible with standard fibre-optic lines, these structures may replace bulky components in sensors, gyroscopes & other devices. While researchers are still probing the unusual properties of the new fibre, tests show the strands impart a chiral, or "handed," character to light by polarizing photons according to certain physical properties. In conventional optical fibres, light is transmitted from one end to the other through a round core housed within a concentric outer cladding. But, because a circular core does not develop handedness when twisted, the research team wound rectangular-core fibres to create a double helix & discovered that some photons left the core & entered the cladding.

Author
Un-named
Origin
Unknown
Journal Title
Am Ceram Soc Bull 83 9 2004 19, 22
Sector
Glass Fibre
Class
GF 425

Request article (free for British Glass members)

Spiraling Glass Fibres
Am Ceram Soc Bull 83 9 2004 19, 22
GF 425
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.