Spinellisation Study Of Three Different Mgo-Al2O3 Compositions Using A Dilatometer

Three different MgO-Al2O3 spinel compositions having MgO: Al2O3 molar ratios 2: 1, 1: 1 and 1: 2 have been studied. Isostatically pressed green compacts of oxide mixtures were used for the dilatometric study and a maximum temperature of 1400 deg C was used. Dilatometric study reveals that the formation of spinel starts above 1000 deg C for all the compositions and the linear expansion values are in good agreement with their expected values considering theoretically possible spinel content. The fall in expansion values was also observed and above 1350 deg C due to greater shrinkate rate, from sintering, than the rate of expansion from spinellisation. The phase analyses of the final products showed spinel as the major phase with some free oxides due to incomplete spinellisation reaction.

Author
R Sarkar Et Al
Origin
Central Glass & Ceramic Research, India
Journal Title
Trans Ind Ceram Soc 61 4 Oct-Dec/02 173-175
Sector
Refractories
Class
R 527

Request article (free for British Glass members)

Spinellisation Study Of Three Different Mgo-Al2O3 Compositions Using A Dilatometer
Trans Ind Ceram Soc 61 4 Oct-Dec/02 173-175
R 527
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
14 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.