Spinel Bricks For Highly Stressed Roofs In Glass Melting Furnaces

New challenges are raised to refractory materials in the crown and superstructure of oxy-fuel fired glass melting furnaces in comparison to air-fuel fired glass melting furnaces. In glass melting furnaces which are oxy-fuel fired, the water steam partial pressure above the melt increases very strongly. In the case of soda-lime-silica glass melts together with the water steam partial pressure the alkaline hydroxide partial pressure increases with a factor of three in comparison to an air-fuel firing system. This leads to an aggressive action on the refractory lining in the crown and superstructure. After extensive thermodynamic calculations and laboratory tests a pure spinel refractory material (MgO.Al203) was developed for the application in the crown and superstructure of oxy-fuel fired glass melting furnaces.

Author
G Boymanns Et Al
Origin
Vesuvis, Germany
Journal Title
Glastech Ber Glass Sci Technol 73 10 2000 293-298
Sector
Refractories
Class
R 370

Request article (free for British Glass members)

Spinel Bricks For Highly Stressed Roofs In Glass Melting Furnaces
Glastech Ber Glass Sci Technol 73 10 2000 293-298
R 370
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.