Spectroscopy Of Sm3+ Ion In Calcium Metaphosphate Glass

Optical absorption and photoluminescence characteristics for Sm3+ ions doped in the range 8.7x1019 to 7.8x1020 ions cm-3 in calcium metaphosphate glasses are presented.