Spectroscopic Properties And Local Structure Of Eu3+ In Ge-Ga-S-Csbr (Or Cscl) Glasses

Spectroscopic properties and local structure of Eu3+ in Ge-Ga-S-CsBr (or CsSl) glasses were investigated using fluorescence measurements and several spectroscopic methods.

Author
W Chung & J Heo
Origin
Photonic Glass Labs, University Science/Technol, S Korea
Journal Title
J Am Ceram Soc 86 2 2003 286-290