Spectroscopic Investigations Of The Er3+ Fluorescence Transitions At 540Nm And 1.5Um In Fluoride Phosphate And Phosphate Glasses

Fluoride phosphate glasses with different phosphate contents and metaphosphate glasses, both with different Er3+ concentrations of 3 to 10.1019cm-3, were prepared. The lifetimes and the intensities of the fluorescence transitions 4S3/2 > 4I15/2 at 540nm and 4I13/2 > 4I15/2 at 1.5um have been studied as a function of phosphate content and Er3+ concentration.

Author
H Ebendorff-Heidepriem Et Al
Origin
Friedrich-Schuller University, Germany
Journal Title
Glastech Ber 66 9 1993 235-244
Sector
Special Glass
Class
S 764

Request article (free for British Glass members)

Spectroscopic Investigations Of The Er3+ Fluorescence Transitions At 540Nm And 1.5Um In Fluoride Phosphate And Phosphate Glasses
Glastech Ber 66 9 1993 235-244
S 764
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
15 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.