Spectroscopic Characterization Of Nickel In Borate And Silicate Glasses

Optical absorption spectroscopy and colorimetric analysis have been used to provide information on the relation between the sites distribution of Ni2+ and the colour of nickel-bearing alkali borate and silicate glasses.

Author
L Galoisy, G Calas
Origin
University Of Paris
Journal Title
Riv Staz Sper Vetro 1990 20 5 33-37