Spectrophotometric Determination Of Visible & Solar Parameters Of Sand-Blasted Glass Panes & Translucent Glass Laminates

The Technical Committee on "Optical Properties of Glass" of the International Commission on Glass (ICG-TC10) organised Round Robins on normal incidence transmittance & reflectance measurements on translucent glass panes in the solar range using commercial spectrophotometers equipped with integrating sphere accessories. The samples were sand-blasted glass panes & glass laminates with translucent plastic films representative of the current production. The measures of visible & solar parameters were then obtained from the recorded spectral curves following the procedures established by the European standard EN410. The recorded curves &, consequently, the integrated values showed large discrepancies & underestimated the parameters due to the inappropriate geometry of the small integrating spheres used in commercial spectrometers.

Author
P Polato Et Al
Origin
Unknown
Journal Title
Rivista Staz Sper Vetro 33 5 2003 5-18
Sector
Flat glass
Class
F 2488

Request article (free for British Glass members)

Spectrophotometric Determination Of Visible & Solar Parameters Of Sand-Blasted Glass Panes & Translucent Glass Laminates
Rivista Staz Sper Vetro 33 5 2003 5-18
F 2488
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.